Atomic layer deposition and in situ characterization of ultraclean lithium oxide and lithium hydroxide

Alexander C. Kozen, Alexander J. Pearse, Chuan Fu Lin, Marshall A. Schroeder, Malachi Noked, Sang Bok Lee, Gary W. Rubloff